Lead paste and lead contented material after desulfurization will be feeding into rotary furnace by screw conveyor and vibrator feeder continuously. The smelting temperature is below 1100℃, after the slurry layer interaction and Chromatography stationary, lead liquid will flow out. And the Oxide slag in the furnace accumulating to a certain amount it will flow out also.